- Mineral Resources
- Online Spatial Data
- Alaska Geochemical Database
AGDB measured parameter: Fe2O3_pct_TT_Fuse
Ferric iron, as iron trioxide, in weight percent, by titration after fusion
Reference for the analytical method
Author |
Baedecker, Philip A., editor |
Year |
1987 |
Title |
Methods for geochemical analysis |
Series |
Bulletin |
Issue |
1770 |
Pages |
1 v.: ill.; 28 cm |
URL |
http://pubs.er.usgs.gov/publication/b1770 |
Notes |
Includes bibliographies. Analytical methods used in the Geologic Division laboratories of the U.S. Geological Survey for the inorganic chemical analysis of rock and mineral samples. |
Organization |
USGS-BAL |
Other parameters measuring Fe2O3
Parameter |
Description |
Fe2O3_pct_AES_Fuse |
Ferric iron, as iron trioxide, in weight percent, by inductively coupled plasma-atomic emission spectroscopy after LiBO2 or LiBO2-Li2B4O7 fusion |
Fe2O3_pct_CM_Fuse |
Ferric iron, as iron trioxide, in weight percent, by spectrophotometry after NaOH or LiBO2-Li2B4O7 fusion, computed as FeTO3 less FeO |
Fe2O3_pct_TT_Fuse |
Ferric iron, as iron trioxide, in weight percent, by titration after fusion |