Field | Value |
---|---|
Unique Sample ID Number | M171779 |
Analytical Job Number | LQ31 |
Submitter Name | Ford, Arthur B. |
Date Submitted | 19860501 |
Field Number | 84AF113A |
State | AK |
Latitude | 58.88639 |
Longitude | -135.09528 |
Source of Sample | outcrop |
Collection Method | single/grab |
Primary Classification | rock |
Secondary Classification | metamorphic |
Specific Name | greenstone |
Additional Attributes and Comments | not metasomatic; quartz unknown; mafic (greenstone, greenschist, amphibolite);; greenstone; |
Stratigraphic Unit Name | UNNAMED (LIONS HEAD MTN) |
Type of Metamorphism | regional |
Metamorphic Facies or Grade | low grade |
(click for info) | |
Geologic map unit | -135.09528, 58.88639 |
Nearby scientific data | Find additional scientific data near this location |
Element | Measured value | Units of measure | Analytical method |
---|---|---|---|
LOI | 2.72 | percent by weight | (unknown method) |
H2O+ | 3.19 | percent bound water | (unknown method) |
H2O- | 0.16 | percent moisture | (unknown method) |
CO2 | 0.52 | percent by weight | Titration |
Sodium | 2.41 | percent by weight | INAA |
Na2O | 2.86 | percent by weight | XRF |
MgO | 8.51 | percent by weight | XRF |
Al2O3 | 12.1 | percent by weight | XRF |
SiO2 | 46.2 | percent by weight | XRF |
P2O5 | 0.19 | percent by weight | XRF |
K2O | 0.22 | percent by weight | XRF |
CaO | 8.44 | percent by weight | XRF |
Scandium | 48.2 | ppm by weight | INAA |
51 | ppm by weight | E-Spec | |
TiO2 | 2.85 | percent by weight | XRF |
Vanadium | 410 | ppm by weight | E-Spec |
Chromium | 340 | ppm by weight | XRF |
306 | ppm by weight | INAA | |
MnO | 0.24 | percent by weight | XRF |
Iron | 12.1 | percent by weight | INAA |
FeO | 10.48 | percent by weight | Titration |
FeTO3 | 16.3 | percent Fe2O3 by weight | XRF |
Cobalt | 60.5 | ppm by weight | INAA |
56 | ppm by weight | E-Spec | |
Nickel | 140 | ppm by weight | XRF |
Copper | 25 | ppm by weight | XRF |
Zinc | 130 | ppm by weight | XRF |
Rubidium | L10 | ppm by weight | XRF |
10.3 | ppm by weight | INAA | |
Strontium | 95 | ppm by weight | XRF |
Yttrium | 26 | ppm by weight | XRF |
30 | ppm by weight | ICP-AES | |
Zirconium | 120 | ppm by weight | XRF |
173 | ppm by weight | INAA | |
Niobium | 12 | ppm by weight | XRF |
Ruthenium | 0.7 | ppb by weight | Fire Assay |
Rhodium | 0.9 | ppb by weight | Fire Assay |
Palladium | 41 | ppb by weight | Fire Assay |
Antimony | L0.13 | ppm by weight | INAA |
Cesium | 0.12 | ppm by weight | INAA |
Barium | 65 | ppm by weight | XRF |
90.5 | ppm by weight | INAA | |
Lanthanum | L30 | ppm by weight | XRF |
8.42 | ppm by weight | INAA | |
8.5 | ppm by weight | ICP-AES | |
Cerium | 30 | ppm by weight | XRF |
22.5 | ppm by weight | INAA | |
21.9 | ppm by weight | ICP-AES | |
Praseodymium | 3 | ppm by weight | ICP-AES |
Neodymium | 16.5 | ppm by weight | INAA |
16.3 | ppm by weight | ICP-AES | |
Samarium | 5.17 | ppm by weight | INAA |
5 | ppm by weight | ICP-AES | |
Europium | 1.79 | ppm by weight | INAA |
1.72 | ppm by weight | ICP-AES | |
Gadolinium | 6.5 | ppm by weight | ICP-AES |
Terbium | 1.04 | ppm by weight | INAA |
1 | ppm by weight | ICP-AES | |
Dysprosium | 6 | ppm by weight | ICP-AES |
Holmium | 1.21 | ppm by weight | ICP-AES |
Erbium | 3.3 | ppm by weight | ICP-AES |
Thulium | 0.44 | ppm by weight | ICP-AES |
Ytterbium | 3.19 | ppm by weight | INAA |
2.6 | ppm by weight | ICP-AES | |
Lutetium | 0.47 | ppm by weight | INAA |
0.34 | ppm by weight | ICP-AES | |
Hafnium | 3.84 | ppm by weight | INAA |
Tantalum | 0.685 | ppm by weight | INAA |
Iridium | L0.5 | ppb by weight | Fire Assay |
Platinum | 9.8 | ppb by weight | Fire Assay |
Gold | L0.1 | ppm by weight | AA |
Thorium | 0.831 | ppm by weight | INAA |